材料是废料,工艺是一次成型。The material is waste. The process is a single press.

传统木托盘要经过选料、烘干、锯切、刨光、钉合五道工序,每一道都在损耗木材、增加人工、引入失效点。我们把这一切压缩成一次模压。 A timber pallet passes through grading, kiln drying, sawing, planing and nailing — each step wasting wood, adding labour and introducing failure points. We compress all of it into one press cycle.

原料来源Feedstock

三类别人打算烧掉的东西。 Three streams other people plan to burn.

不新增一棵树的砍伐指标,只把已经离开森林和工厂的木质剩余物重新变成产品。原料来源可追溯、可按批次出具说明。 We add no felling quota. We take wood residues that have already left the forest and the mill and turn them back into a product. Sources are traceable and documented per batch.

01

采伐剩余物Logging residues

枝桠、树梢、树皮、树根、藤条及灌木——留在山上的部分,过去基本是清林焚烧。Branches, tops, bark, roots, vines and shrubs left on site — historically cleared and burned.

枝桠树皮灌木
02

造材与加工剩余物Mill residues

造材截头、板条、板皮、锯末、碎单板——木材加工厂每天产生、按吨处理的部分。Trimming ends, slabs, edging, sawdust and veneer scrap — the daily tonnage every mill pays to dispose of.

锯末板皮碎单板
03

木质废弃物Post-consumer wood

废弃板材、旧家具、报废木托盘——回收渠道分散,但恰恰是城市里最容易集中的木质资源。Discarded panels, old furniture, retired timber pallets — fragmented collection, but the most concentrated wood resource in a city.

旧家具废板材旧托盘

原料的含水率、杂质与纤维长度直接影响成品强度,因此每一批进厂都要过筛分与含水率检测,不合格的批次不投料。 Moisture content, contamination and fibre length drive finished strength, so every incoming batch is screened and moisture-tested. Failing batches are not fed to the line.

工艺流程Process

五步,从废料到托盘。Five steps from offcut to pallet.

01

收集与分选Collect and sort

按来源分类进厂,剔除金属、砂石与胶合板等异质材料。Sorted by source on arrival; metal, grit and foreign board are removed.

02

破碎与干燥Chip and dry

破碎到工艺粒径后干燥到目标含水率,保证成型时不产生气泡与分层。Reduced to process particle size and dried to target moisture so the part forms without voids or delamination.

03

配混Blend

与环保胶黏体系按比例混合,搅拌均匀度决定每一批的强度一致性。Mixed with a low-emission binder; blend uniformity is what makes batch-to-batch strength repeatable.

04

高温高压成型Press

定量投料进入加热模具,一次加压成型出完整托盘,包括脚墩与加强筋。A weighed charge enters the heated mould and one press cycle yields the complete pallet — feet and ribs included.

05

修边与检验Trim and inspect

去飞边、量尺寸、抽检外观与载重,合格批次入库并留样。Deflashing, dimensional check, appearance and load sampling. Passed batches are stocked with retained samples.

为什么一次成型重要Why one piece matters

失效点少了,寿命就长了。Fewer failure points, longer life.

  • 没有钉子,就不会松No nails to work loose 木托盘最常见的失效是钉合处松动、板条脱落,整托报废。The classic timber failure is a loosened nail or a dropped board that scraps the whole pallet.
  • 没有拼缝,就不会开裂No seams to split 实木拼板在干湿循环下沿胶线开裂,模压件是连续材料。Glued timber splits along its glue lines under wet-dry cycling; a moulded part is continuous material.
  • 没有毛刺,不伤包装No splinters to cut film 缠膜与纸箱不会被木刺划破,出口到货破损率下降。Stretch film and cartons are not punctured, so arrival damage drops.
TIMBER · JOINED ✕ glue line splits · nails loosen MOLDED · ONE PIECE ✓ continuous material, no joints PROCESS STEPS Timber: grade → kiln → saw → plane → nail Molded: chip → dry → blend → press Nail joints zero
拼板结构与一次成型对比示意Joined timber vs. one-piece moulding

材料性能Material properties

七条我们能讲清楚的性能。 Seven properties we can explain.

下面每一条都对应一个可测项。谈技术时我们只讲这些,不讲“颠覆行业”。 Each line below maps to something measurable. This is the full technical claim — no "disrupting the industry".

耐高低温Temperature range

设计工作区间 −40 ℃ 至 60 ℃,覆盖冷库到集装箱内高温。Design window −40 °C to 60 °C, covering cold stores through container heat.

防水防潮Water resistance

整体密闭成型,不吸水、不发霉,可水洗清洁。Closed moulding: no water uptake, no mould, washable.

力学强度Mechanical strength

加强筋与脚墩一次成型,抗弯刚度可通过底架结构调节。Ribs and blocks form in the same cycle; stiffness is tuned by base structure.

尺寸稳定Dimensional stability

不随湿度胀缩,托盘池与自动线的尺寸一致性优于木材。No humidity-driven swelling, so pool and conveyor consistency beats timber.

耐腐蚀Corrosion resistance

对常见酸碱盐雾不敏感,化工与沿海场景可用。Unaffected by common acids, alkalis and salt spray — usable in chemical and coastal sites.

可嵌 RFIDRFID-ready

成型时预留芯片嵌槽,芯片被封在材料内部,不脱落。A cavity is moulded in so the tag sits inside the material and cannot fall out. 需确认模具Tool-dependent

环保与合规Environmental compliance

原料为可再生废料;成品可粉碎再生成型;出口无需熏蒸。有害物质与 VOC 指标以第三方报告为准,目前待送检,不提前承诺数值。Renewable waste feedstock, regrindable at end of life, no export fumigation. Hazardous-substance and VOC figures will come from third-party reports — currently pending, and we do not pre-announce numbers.

我们不承诺什么What we do not claim

不做 3 t 以上动载;不做长期户外无遮蔽暴晒;不做食品直接接触面而未出具专项报告。No dynamic load above 3 t; no long-term uncovered outdoor exposure; no direct food contact without a dedicated report.